Chromium-based BCC-superalloys reinforced by B2-CoAl intermetallic precipitates
Introduces B2-CoAl as an alternative strengthening phase for Cr-based BCC-superalloys, showing slower precipitate coarsening than the Ni-Al analogue and peak hardness of 842 HV at …